ASTM B673 Stainless Steel 904L Seamless Pipe
Feb 05, 2026
Pustite sporočilo
What is 904L stainless steel pipe?
904L (UNS N08904) is a high-alloy austenitic stainless steel containing approximately 19-23% chromium, 23-28% nickel, 4-5% molybdenum, and copper, offering excellent resistance to pitting corrosion, crevice corrosion, and aggressive chemical environments (including strong acids and chloride-rich media). This makes it ideal for chemical, petrochemical, and marine applications requiring long-term durability.
If you are looking for high-performance, corrosion-resistant piping solutions, we offer high-quality, reliably delivered ASTM B673 904L stainless steel seamless pipes, widely used in chemical plants, desalination plants, heat exchangers, offshore oil and gas pipelines, pharmaceutical production, and high-purity fluid systems.

Our ASTM B673 904L seamless pipes are manufactured using processes such as vacuum induction melting, hot extrusion, cold drawing or hot rolling, solution annealing, and pickling, ensuring a dense, defect-free microstructure, uniform wall thickness, and precise dimensional tolerances. Product forms include ASTM B6673 904L seamless round tubes, ASTM B673 904L thick-walled tubes, ASTM B673 904L precision cut tubes, and ASTM B673 904L custom diameter tubes. Surface treatments include polishing, pickling, or bright annealing, with typical hardness controlled at <=220 HB to ensure optimal machinability and formability.
Specification List of Stainless Steel 904L Pipe
| ASTM B673, B677 / ASME SB673, SB 677 | |
| 1/2 – 16″ NB | |
| 1/2 – 24″ NB | |
| 6 – 100″ NB | |
| 1/8 TO 30″NB IN | |
| < Chart/td> | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
Composition Standard of B673 TP 904L Welded Pipes
| C | P | S | |||||||
| SS 904L | 0.020 max | 2.00 max | 1.00 max | 0.040 max | 0.030 max | 19.00 - 23.00 | 4.00 - 5.00 max | 23.00 - 28.00 | 1.00 - 2.00 |
Mechanical Analysis of ASTM B673 TP 904L Pipe
| Yield Strength (0.2%Offset) | ||||
| 7.95 g/cm3 | 1350 ℃ (2460 ℃F) | Psi - 71000 , MPa - 490 | Psi - 32000 , MPa - 220 | 35 % |
Stainless Steel 904L Pipe Wall Thickness & Length
| 1/8" ~ 8" | SCH 5 / SCH 10 / SCH 40 / SCH 80 / SCH 160 | Upto 6 Meters | |
| Nickel 201 Seamless Pipe (Custom Sizes) | 5.0mm ~ 203.2mm | Upto 6 Meters | |
| Nickel 201 Welded Pipe (in Stock + Custom Sizes) | 5.0mm ~ 1219.2mm | 1.0 ~ 15.0 mm | Upto 6 Meters |
Application of Stainless Steel 904L Pipe
Chemical Processing Industry: Widely used in equipment handling aggressive acids (sulfuric, phosphoric, acetic, formic) due to its high nickel and molybdenum content.
Oil & Gas Industry: Utilized in subsea pipelines, offshore rigs, and refineries for transporting corrosive, high-chloride materials.
Marine & Seawater Applications: Ideal for seawater cooling systems, condenser tubes, and offshore processing equipment because of its resistance to pitting and crevice corrosion.
Pollution Control: Used in gas scrubbing systems and flue gas desulfurization (FGD) plants in coal-fired power stations to handle corrosive fumes and wet gases.
Pulp and Paper Industry: Employed in bleaching plants and digestion systems due to resistance to chloride attacks.
| Price list of Stainless Steel 904L Pipe | SUS 904L Pipe Price in USD |
|---|---|
| SS 904L Hollow Pipe Size:235mm Odx 120mm Id X 235mm Long | 2549.14 USD |
| 904L grade stainless steel seamless cold-drawn tubes | $4.66 |
We ensure product quality through comprehensive chemical and mechanical property testing, tensile and impact analysis, dimensional inspection, surface quality control, and non-destructive testing (UT/ET). Each batch of products is accompanied by an EN 10204 3.1 / ASTM B673 material certificate, and third-party inspection is available upon request. With extensive export experience to Europe, North America, the Middle East, and Southeast Asia,