SUS317L Stainless Steel: High-Molybdenum Corrosion Resistance
Jan 20, 2026
Pustite sporočilo



The chemical composition of grade 317L stainless steel is outlined in the following table.
| 18-20 | |
| 11-15 | |
| 3-4 | |
| 2 | |
| 1 | |
| 0.045 | |
| 0.03 | |
| 0.03 |
The mechanical properties of grade 317L stainless steel are displayed in the following table.
| 595 MPa | 86300 psi | |
| 260 MPa | 37700 psi | |
| 200 GPa | 29000 ksi | |
| 0.27-0.30 | 0.27-0.30 | |
| Elongation at break (in 50 mm) | 55% | 55% |
| 85 | 85 |
Naslednji: 1,4410 ekvivalent materiala astm
Pošlji povpraševanje