316 Stainless Steel: The Molybdenum-Added Corrosion-Resistant Grade
Dec 22, 2025
Pustite sporočilo
316 stainless steel is the molybdenum-bearing austenitic grade based on the 18-8 chromium-nickel system. The defining difference from 304 is the addition of 2.00-3.00% molybdenum, which strengthens the passive film and makes the grade markedly more resistant to pitting and crevice corrosion in chloride ion environments. As a result, 316 is the standard selection for marine hardware, chemical process equipment and food processing plant where 304 would be at risk of localized attack.
Chemical composition (ASTM A240, wt%)
| 0.08 max | |
| 1.00 max | |
| 2.00 max | |
| 0.045 max | |
| 0.030 max | |
| 16.00 - 18.00 | |
| 10.00 - 14.00 | |
| 2.00 - 3.00 |
For plate in the solution-annealed condition, ASTM A240 requires a minimum tensile strength of 515 MPa, a minimum yield strength of 205 MPa and a minimum elongation of 40%; the annealed Brinell hardness is typically 217 HB max. The grade retains good toughness down to cryogenic temperatures (about -196℃C) and can be used in continuous service up to approximately 870℃C where oxidation resistance governs.
| 515 MPa | |
| Yield strength (0.2% offset) | 205 MPa |
| 40% | |
| 217 HB max |
Molybdenum enriches the passive oxide film and suppresses the initiation and growth of metastable pits in chloride solutions. The improvement is expressed by the pitting resistance equivalent number, PREN=Cr + 3.3Mo + 16N, which for 316 is approximately 24-26 versus about 18-20 for 304. The practical result is that 316 tolerates higher chloride concentrations and temperatures before pitting and crevice corrosion initiate.
The family includes the low-carbon variant 316L (UNS S31603, carbon 0.030% max) for welded construction, and the high-carbon variant 316H (UNS S31609, carbon 0.04-0.10%) for elevated-temperature strength. Equivalent designations: JIS SUS316, EN 1.4401 (X5CrNiMo17-12-2), GB 06Cr17Ni12Mo2.
Typical applications include marine components and offshore platform equipment, chemical reactors and chloride-bearing process piping, heat exchangers and condensers, food and beverage processing equipment, desalination plant components, medical device components (the low-carbon 316L variant) and coastal architectural structures.
Q1: What is the core difference between 316 and 304? A1: The molybdenum content. 316 contains 2.00-3.00% molybdenum, which raises pitting resistance (PREN about 24-26) well above that of 304, and 316 also has a higher nickel range of 10.00-14.00%.
Q2: Can 316 be used in seawater? A2: It is widely used in marine environments and can serve in ambient seawater service with appropriate design; for warm, stagnant or highly creviced seawater service, higher-alloyed grades should be evaluated.
Q3: Why is 316 more expensive than 304? A3: The main cost driver is alloy content: 2.00-3.00% molybdenum plus a higher nickel range (10.00-14.00% versus 8.00-10.50% for 304) increase raw material cost.
Q4: Is 316 suitable for low-temperature service? A4: Yes, the austenitic structure keeps high impact toughness down to about -196℃C, making 316 suitable for cryogenic storage and handling equipment when welding is controlled to maintain soundness.
Q5: How is a locally corroded 316 surface repaired? A5: The affected area is ground back to sound metal, weld-repaired with matching or low-carbon molybdenum-bearing filler such as ER316L, dressed smooth, and passivated to restore the protective oxide film.
Pošlji povpraševanje